A coating datasheet says "500 hours salt spray".

Illustration for astm b117 salt spray test: a salt pile, a salt-spray test cabinet and carbide crystals marked WC
4 answersAsked 24 October 2026·Materials & Standards

SENTHAI Editorial Team

TALK / MATERIALS AND STANDARDS DISCUSSION
Buyer question

A bolt supplier quotes salt-spray hours. Does a higher number mean our plow hardware will last longer on salted roads?

Scenario: a coating datasheet says “500 hours salt spray”. Direct answer: that number describes how a specimen behaved in a defined test chamber. It is not a number of winters. ASTM B117 itself says so in plain terms.

What the standard says about itself

The standard describes its own scope, and that scope is narrower than most buyers assume.

  • Scope (1.1, 1.2): the practice covers the apparatus, procedure and conditions needed to create and maintain a salt spray (fog) environment. It does not prescribe the type of specimen, the exposure period for a given product or how to interpret the results.
  • Use (3.1): it provides a controlled corrosive environment used to produce relative corrosion-resistance information for metals and coated metals in a given chamber.
  • Limits (3.2): prediction of performance in natural environments has seldom been correlated with salt spray results used as stand-alone data, and correlation or extrapolation is not always predictable.
  • Repeatability (3.3): results depend heavily on specimen type, evaluation criteria and control of operating variables, and variability has been observed between chambers.

I read the current B117-26a store page (updated September 22, 2026). The full text is paid, so I cite only the public scope and significance text.

What to ask when a supplier quotes hours

Question Why it matters
Which edition of the standard, and which lab? Results vary between chambers
What was tested: bolts, plated nuts or a flat panel? Shape and coating thickness differ
What failure criterion ended the test? “No red rust” and “5% rust” are different results
Was the coating scratched before testing? Plow hardware gets scratched in use
Is there real-world history on a similar part? The standard itself stresses long-term exposure data

An example of the difference

Suppose two suppliers each quote a coating with the same number of hours. One tested a flat panel to first sign of red rust; the other tested threaded bolts to a percentage of rust coverage. The numbers look equal but do not measure the same thing. This is an illustration of how criteria differ, not data about real products.

A practical reading

Hours are only comparable between tests run the same way.

  1. Treat hours as a way to compare two coatings tested the same way, not as a lifetime.
  2. Weigh it against salt-brine exposure, road chemicals and abrasion on your own routes.
  3. Keep a corrosion note in your edge log. Your own trucks are the best long-term test.

Boundary: I make no statement about what any specific plow bolt or coating achieves in chamber hours or in service.

↳ Replying to SENTHAI Editorial Team

If two bolt coatings both quote test hours, check the spec of the test before the number. A shorter test with strict criteria may say more than a longer one that allows substantial rust. Also weigh the hardware’s job: a structural bolt that sees impact needs strength and fit, so corrosion data are only one input, and you should confirm strength grade from the supplier separately.

↳ Replying to Selection perspective

Ask for the full test report, not a datasheet line. A reputable supplier can provide a lab name, date, specimen description and failure criterion. If they cannot, treat the hours as a marketing figure. Request the same documents from each bidder so the comparison between offers is fair and recorded, and file the reports with the purchase order.

↳ Replying to Purchasing perspective

Corrosion in service depends heavily on washing and drying. Salt left on hardware between storms continues to attack it. A rinse routine after salt exposure, and a look at bolts, nuts and washers each week, will usually extend hardware life more than a small difference in test hours, though I have no measured figure to offer on that.

Next step

Scenario: a coating datasheet says “500 hours salt spray”.

Send us a blade drawing and get a quote back